← BackMaterial grade directory

Q345C

4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for Q345C →

Q345C · GB /T 1591-1994

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1591—1994
Table / clause
5.1.1/Table 1 + clauses 5.1.1.1—13
PDF page references
1、3、4
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default heat-composition range in Table 1
IIW / CEV:0.1667–0.5967Known-element contribution; incomplete value; missing Mo; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0500–0.3483Known-element contribution; incomplete value; missing Mo, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1000–0.3975Known-element contribution; incomplete value; missing Mo; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
5.1.1.3 Q345 Mn option raising the maximum to 1.70%
IIW / CEV:0.1667–0.6133Known-element contribution; incomplete value; missing Mo; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0500–0.3533Known-element contribution; incomplete value; missing Mo, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1000–0.4075Known-element contribution; incomplete value; missing Mo; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Mn1.0 ~ 1.6
Si≤ 0.55 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
V0.02 ~ 0.15
Nb0.015 ~ 0.06
Ti0.02 ~ 0.2
Al≥ 0.015 (upper limit not stated)
Cu≤ 0.3 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

Applicability and limitations

GB/T 1591—1994, Table 1; Heat-analysis mass fractions wt%. Requirements from other current editions are not backfilled into this edition. V/Nb/Ti/Al in Table 1 are grain-refining elements; 5.1.1.6—8 requires at least one of C/D/E; A/B is optional and, when not added, is neither analyzed nor guaranteed; All four minima must not be imposed simultaneously as default requirements. For all 5.1.1.10 grades, residual Cr/Ni/Cu are each ≤0.30%; Table 1 of Q390/Q420/Q460 separately lists a Cr/Ni limit; interpret it according to whether the element is intentionally added as an alloying constituent. 5.1.1.4 sheet

hot-rolled strip has a thickness exception for the Mn minimum; The Nb minimum for 5.1.1.9 sections and bars is 0.005%; Special forms and contract conditions require manual review. This standard covers high-strength low-alloy structural steels; This does not establish cold-heading wire suitability, actual supply or a default mechanical-property guarantee. 5.1.1.3 Q345 Mn maximum may be raised to 1.70%; For 5.1.1.5 using Nb with mechanical properties guaranteed, the Q345/Q390 Mn minimum may be below Table 1. Al≥0.015% in Table 1 is total aluminum; In the 5.1.1.6 grain-refining combination, at least one element must meet its corresponding minimum; all elements are not simultaneously mandatory.

Combined limits

Conditional composition lower limit
  • V
  • Nb
  • Ti
  • Al

Original condition-branch records

Default heat-composition range in Table 1

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Mn1.0 ~ 1.6
Si≤ 0.55 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
V0.02 ~ 0.15
Nb0.015 ~ 0.06
Ti0.02 ~ 0.2
Al≥ 0.015 (upper limit not stated)
Cu≤ 0.3 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

5.1.1.3 Q345 Mn option raising the maximum to 1.70%

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Mn1.0 ~ 1.7
Si≤ 0.55 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
V0.02 ~ 0.15
Nb0.015 ~ 0.06
Ti0.02 ~ 0.2
Al≥ 0.015 (upper limit not stated)
Cu≤ 0.3 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Complete 7-page scan of edition 1994; Table 1 has 20 entries; Grain refinement and replacement ranges require manual interpretation.

Q345C · GB/T 1591-2008

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
High-strength low-alloy structural steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1591-2008
Table / clause
Table 1 · continued table · Notes a/b; 6.1.1–6.1.7

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Cr/Ni/Cu are residual elements, each ≤0.30%; Al in the table is acid-soluble aluminum Al(s)
IIW / CEV:0.0000–0.6333 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3583Known-element contribution; incomplete value; missing B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4175 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu are residual elements, each ≤0.30%; Based on total aluminum Al(t)≥0.020%
IIW / CEV:0.0000–0.6333 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3583Known-element contribution; incomplete value; missing B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4175 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Al in the table is acid-soluble aluminum Al(s)
IIW / CEV:0.0000–0.6467 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3617Known-element contribution; incomplete value; missing B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4225 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Based on total aluminum Al(t)≥0.020%
IIW / CEV:0.0000–0.6467 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3617Known-element contribution; incomplete value; missing B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4225 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 1.7 (lower limit not stated)
Nb≤ 0.07 (lower limit not stated)
V≤ 0.15 (lower limit not stated)
Ti≤ 0.2 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Ni≤ 0.5 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
N≤ 0.012 (lower limit not stated)
Mo≤ 0.1 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Al≥ 0.015 (upper limit not stated)

Applicability and limitations

Heat analysis, mass fractions wt%; Retain the identity of the 2008 edition; do not apply the 2018 edition.. ; When grain refining elements need to be added per 6.1.2, at least one of Al/Nb/V/Ti must be contained and specified in the quality certificate.; This clause does not provide mandatory general lower limits for all elements.. ; 6.1.4 When nitrogen-fixing alloying elements such as Al/Nb/V/Ti are added, N is not restricted, but the nitrogen-fixing elements must be specified.; If this condition is not selected, the N upper limit listed in the table is the default.. ; Table 1, Note a: For sections/bars, the P and S limits may each increase by 0.005%; the upper limit for quality class A may be 0.045%.; Cannot be used for other products.. ; Table 1 Note b: When grain refining elements are added in combination, Nb+V+Ti≤0.22% and Mo+Cr≤0.30%.; The individual-element upper limits cannot all be taken simultaneously.. ; Clause 6.1.6: RE is calculated as an addition of 0.02–0.20% of the molten-steel weight, not as guaranteed finished-product composition..

Combined limits

Product-form exception
P
0.005
S
0.005
Class A product-form upper limit
Not stated
Element-sum limits
    Conditional combined limit
    • Elements concerned
      • Nb
      • V
      • Ti
      Upper limit
      0.22
    • Elements concerned
      • Mo
      • Cr
      Upper limit
      0.3
    Nitrogen-fixing exception conditions
    Yes

    Original condition-branch records

    Cr/Ni/Cu are residual elements, each ≤0.30%; Al in the table is acid-soluble aluminum Al(s)

    ElementComposition requirement
    C≤ 0.2 (lower limit not stated)
    Si≤ 0.5 (lower limit not stated)
    Mn≤ 1.7 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    V≤ 0.15 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.3 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.012 (lower limit not stated)
    Mo≤ 0.1 (lower limit not stated)
    P≤ 0.03 (lower limit not stated)
    S≤ 0.03 (lower limit not stated)
    Al≥ 0.015 (upper limit not stated)

    Cr/Ni/Cu are residual elements, each ≤0.30%; Based on total aluminum Al(t)≥0.020%

    ElementComposition requirement
    C≤ 0.2 (lower limit not stated)
    Si≤ 0.5 (lower limit not stated)
    Mn≤ 1.7 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    V≤ 0.15 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.3 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.012 (lower limit not stated)
    Mo≤ 0.1 (lower limit not stated)
    P≤ 0.03 (lower limit not stated)
    S≤ 0.03 (lower limit not stated)
    Al≥ 0.02 (upper limit not stated)

    Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Al in the table is acid-soluble aluminum Al(s)

    ElementComposition requirement
    C≤ 0.2 (lower limit not stated)
    Si≤ 0.5 (lower limit not stated)
    Mn≤ 1.7 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    V≤ 0.15 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.5 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.012 (lower limit not stated)
    Mo≤ 0.1 (lower limit not stated)
    P≤ 0.03 (lower limit not stated)
    S≤ 0.03 (lower limit not stated)
    Al≥ 0.015 (upper limit not stated)

    Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Based on total aluminum Al(t)≥0.020%

    ElementComposition requirement
    C≤ 0.2 (lower limit not stated)
    Si≤ 0.5 (lower limit not stated)
    Mn≤ 1.7 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    V≤ 0.15 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.5 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.012 (lower limit not stated)
    Mo≤ 0.1 (lower limit not stated)
    P≤ 0.03 (lower limit not stated)
    S≤ 0.03 (lower limit not stated)
    Al≥ 0.02 (upper limit not stated)

    A condition branch must be selected

    Yes

    Verification notes

    Original text of Table 1, notes a/b and the applicability conditions in Clause 6.1 checked

    Q345C · GB /T 3274-2017

    Original-source verification is incomplete; this is not a formal standard reference

    Material category
    Alloy steel
    Subcategory
    Alloy steel
    Material form
    Reference record
    Verification status
    Reference data; original source not verified

    Carbon-equivalent reference

    IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
    Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
    CET: composition source not verified; standard-range carbon equivalent is not calculated

    Composition

    ElementComposition requirement
    C≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    Mn≤ 1.7 (lower limit not stated)
    Mo≤ 0.1 (lower limit not stated)
    N≤ 0.012 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    Ni≤ 0.5 (lower limit not stated)
    P≤ 0.03 (lower limit not stated)
    S≤ 0.03 (lower limit not stated)
    Si≤ 0.5 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    V≤ 0.15 (lower limit not stated)

    Applicability and limitations

    A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

    Q345C · GB 6479-2013

    Original-source verification is incomplete; this is not a formal standard reference

    Material category
    Alloy steel
    Subcategory
    Alloy steel
    Material form
    Reference record
    Verification status
    Reference data; original source not verified

    Carbon-equivalent reference

    IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
    Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
    CET: composition source not verified; standard-range carbon equivalent is not calculated

    Composition

    ElementComposition requirement
    C0.12 ~ 0.2
    Cr≤ 0.3 (lower limit not stated)
    Mn1.2 ~ 1.7
    Mo≤ 0.1 (lower limit not stated)
    Nb≤ 0.07 (lower limit not stated)
    Ni≤ 0.5 (lower limit not stated)
    P≤ 0.025 (lower limit not stated)
    S≤ 0.015 (lower limit not stated)
    Si0.2 ~ 0.5
    V≤ 0.15 (lower limit not stated)

    Applicability and limitations

    A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

    WhatsApp Technical enquiry →