POSWELD1B
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for POSWELD1B →POSWELD1B · POSCO wire rod catalogue (local archive 1203; original edition not stated)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Local file 1203 (wire-rod pdf); the original does not state a publication edition; PDF metadata 2014-12-03 is only the file generation time
- Document title
- Wire rod
- Table / clause
- Printed page 25, composition table 5 (local table index)
- PDF page references
- 13
- Unit
- Percentages as stated in the original table; refer to the source for the specific basis
- Analysis type
- The catalog does not consistently specify heat or product analysis
- Manufacturer
- POSCO
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Si | 0.4 ~ 1.0 |
| Mn | 1.0 ~ 1.6 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Al | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
POSCO local wire rod catalogue, PDF page 13
printed page 25, table index 4, row 2. The original edition number is not stated; the PDF creation date 2014-12-03 is not the standard publication year. Manufacturer range information does not constitute our supply guarantee. The remark specifies Ti+Zr≤0.13%; do not split into independent limits. Welding-wire remark columns were added from the original images; this is not automatic recognition of blanks beyond 7 columns.
Composition conditions
- Original catalog chemical composition table %, wire rod; Editions of JIS/SAE/DIN were not provided; catalog data shall not be upgraded to the verified official editions of these standards.
- Dashes are not zero; cast/product analysis types are not consistently explicit. Orders, product-analysis deviations and actual supply require separate verification.
- Remark specifies Ti+Zr≤0.13%; do not split this into individual limits.
- Supplementary welding wire/wire rod entries under Remark were added from the original image; they are not automatically inferred blanks beyond the 7 columns.
Combined limits
- Element-sum limits
- Elements concerned
- Ti
- Zr
- Upper limit
- 0.13