Open condition selection, comparison and carbon-equivalent tools for POSMA45R →POSMA45R · POSCO wire rod catalogue (local archive 1203; original edition not stated)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Local file 1203 (wire-rod pdf); the original does not state a publication edition; PDF metadata 2014-12-03 is only the file generation time
- Document title
- Wire rod
- Table / clause
- Printed page 27, composition table 5 (local table index)
- PDF page references
- 14
- Unit
- Percentages as stated in the original table; refer to the source for the specific basis
- Analysis type
- The catalog does not consistently specify heat or product analysis
- Manufacturer
- POSCO
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.43 ~ 0.47 |
| Si | 0.2 ~ 0.4 |
| Mn | 1.1 ~ 1.5 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.06 (lower limit not stated) |
| S-Al | 0.01 ~ 0.07 |
| Ni | ≤ 0.2 (lower limit not stated) |
| V | ≤ 0.11 (lower limit not stated) |
| N | ≤ 0.015 (lower limit not stated) |
Applicability and limitations
POSCO local wire rod catalogue, PDF page 14
printed page 27, table index 4, row 2. The original edition number is not stated; the PDF creation date 2014-12-03 is not the standard publication year. Manufacturer range information does not constitute our supply guarantee. S-Al is retained as a separate original-table column, not merged with total Al. Original N maximum 150ppm; 1%=10000ppm. Units converted without changing the one-sided limit.
Composition conditions
- Original catalog chemical composition table %, wire rod; Editions of JIS/SAE/DIN were not provided; catalog data shall not be upgraded to the verified official editions of these standards.
- Dashes are not zero; cast/product analysis types are not consistently explicit. Orders, product-analysis deviations and actual supply require separate verification.
- S-Al is retained separately as in the original column and is not merged with total Al.
- Original N(ppm) value: 150 Max.; 1%=10000ppm, converted according to units, single-sided limits remain unchanged.