P265GH
10 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for P265GH →P265GH · EN 10028-2-2009
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≥ 0.02 (upper limit not stated) |
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.02 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.03 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · EN 10028-2-2017
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≥ 0.02 (upper limit not stated) |
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.03 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.03 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · EN 10216-2-2024
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≥ 0.02 (upper limit not stated) |
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.02 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.04 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · EN 10217-2-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · EN 10217-5-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · EN 10222-2-2017
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | 0.5 ~ 1.4 |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.01 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.03 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · NF EN 10216-2-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · NF EN 10217-2-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.02 (lower limit not stated) |
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.01 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.03 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · NF EN 10253-2-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 1.4 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
P265GH · ISO 9328-2-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.02 (lower limit not stated) |
| C | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | 0.8 ~ 1.4 |
| Mo | ≤ 0.08 (lower limit not stated) |
| N | ≤ 0.012 (lower limit not stated) |
| Nb | ≤ 0.02 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.03 (lower limit not stated) |
| V | ≤ 0.02 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.