NIMO28
6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for NIMO28 →NiMo28 · DIN 17744-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.08 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiMo28 · DIN 17744-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.08 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiMo28 · DIN 17750-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Classification basis (does not replace original-source composition verification)
The titles of the listed standards are nickel and nickel alloy electrodes, welding wires, forgings, or sheet and strip materials; Only the classification field is corrected; the verification status of the original chemical composition text remains unchanged.
GB/T15620-2008 Nickel and nickel alloy welding wires
GB/T13814-2008 Nickel and nickel alloy electrodes
GB/T26030-2010 Nickel and nickel alloy forgings
DIN17750:2002 Bänder und Bleche aus Nickel und Nickel-Knetlegierungen
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.08 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiMo28 · DIN 17750-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Classification basis (does not replace original-source composition verification)
The titles of the listed standards are nickel and nickel alloy electrodes, welding wires, forgings, or sheet and strip materials; Only the classification field is corrected; the verification status of the original chemical composition text remains unchanged.
GB/T15620-2008 Nickel and nickel alloy welding wires
GB/T13814-2008 Nickel and nickel alloy electrodes
GB/T26030-2010 Nickel and nickel alloy forgings
DIN17750:2002 Bänder und Bleche aus Nickel und Nickel-Knetlegierungen
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.08 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiMo28 · DIN 17752-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.08 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiMo28 · GB /T 26030-2010
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Classification basis (does not replace original-source composition verification)
The titles of the listed standards are nickel and nickel alloy electrodes, welding wires, forgings, or sheet and strip materials; Only the classification field is corrected; the verification status of the original chemical composition text remains unchanged.
GB/T15620-2008 Nickel and nickel alloy welding wires
GB/T13814-2008 Nickel and nickel alloy electrodes
GB/T26030-2010 Nickel and nickel alloy forgings
DIN17750:2002 Bänder und Bleche aus Nickel und Nickel-Knetlegierungen
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | ≤ 1 (lower limit not stated) |
| Fe | ≤ 2 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | 26 ~ 30 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.