NiCr29Fe · DIN 17742-2002

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.5 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Cr27 ~ 31
Cu≤ 0.5 (lower limit not stated)
Fe7 ~ 11
Mn≤ 0.5 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Ti≤ 0.5 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

NiCr29Fe · DIN 17742-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.5 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Cr27 ~ 31
Cu≤ 0.5 (lower limit not stated)
Fe7 ~ 11
Mn≤ 0.5 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Ti≤ 0.5 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

NiCr29Fe · DIN 17750-2002

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.5 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Cr27 ~ 31
Cu≤ 0.5 (lower limit not stated)
Fe7 ~ 11
Mn≤ 0.5 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Ti≤ 0.5 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

NiCr29Fe · DIN 17752-2002

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.5 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Cr27 ~ 31
Cu≤ 0.5 (lower limit not stated)
Fe7 ~ 11
Mn≤ 0.5 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Ti≤ 0.5 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

NiCr29Fe · EN 10302-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.5 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Cr27 ~ 31
Cu≤ 0.5 (lower limit not stated)
Fe7 ~ 11
Mn≤ 0.5 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)

Applicability and limitations