NICR22MO9NB
9 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for NICR22MO9NB →NiCr22Mo9Nb · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Subcategory
- Special alloy steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 3,footnotes 1/2;7.2
- PDF page references
- 1、2、3、9、17
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.03 ~ 0.1 |
| Mn | ≤ 0.5 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Ni | ≥ 58.0 (upper limit not stated) |
| Cr | 20.0 ~ 23.0 |
| Co | ≤ 1.0 (lower limit not stated) |
| Fe | ≤ 5.0 (lower limit not stated) |
| Mo | 8.0 ~ 10.0 |
| Al | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply.
Combined limits
- Combined-element limits
- Element coefficient
- Nb
- 1
- Ta
- 1
- Requirement
- Combined Nb+Ta 3.15–4.15%
- Lower limit
- 3.15
- Upper limit
- 4.15
- Elements requiring measured values from the same heat
- Nb
- Ta
Verification notes
Official original DIN EN 10095:2018-12 composition and footnotes have been checked; Spacing within grade designations is normalized for correspondence; the EN year and DIN correction date are retained separately.NiCr22Mo9Nb · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 3,footnotes 1/2;7.2
- PDF page references
- 1、2、3、9、17
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.03 ~ 0.1 |
| Mn | ≤ 0.5 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Ni | ≥ 58.0 (upper limit not stated) |
| Cr | 20.0 ~ 23.0 |
| Co | ≤ 1.0 (lower limit not stated) |
| Fe | ≤ 5.0 (lower limit not stated) |
| Mo | 8.0 ~ 10.0 |
| Al | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply.
Combined limits
- Combined-element limits
- Element coefficient
- Nb
- 1
- Ta
- 1
- Requirement
- Combined Nb+Ta 3.15–4.15%
- Lower limit
- 3.15
- Upper limit
- 4.15
- Elements requiring measured values from the same heat
- Nb
- Ta
Verification notes
All 26 chemical-composition rows and applicable footnotes in the official German text dated 2018-12 were checked; the 2018 corrigendum and product-analysis deviations are recorded separately.NiCr22Mo9Nb · EN 10095-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10095:1999
- Table / clause
- Table 3 and footnotes; complete historical original edition
- PDF page references
- 1、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.03 ~ 0.1 |
| Mn | ≤ 0.5 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Ni | ≥ 58.0 (upper limit not stated) |
| Cr | 20.0 ~ 23.0 |
| Co | ≤ 1.0 (lower limit not stated) |
| Fe | ≤ 5.0 (lower limit not stated) |
| Mo | 8.0 ~ 10.0 |
| Al | ≤ 0.4 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
| Cu | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
Original historical EN 10095:1999, Table 1—3 gives heat-analysis mass fractions wt%; This source is a scan of that original edition and must not be identified as DIN EN 10095:2018-12. ; Unlisted elements are not treated as zero and must not be intentionally added without purchaser consent, except additions needed to finish steelmaking. ; Specific supply form, heat treatment, properties and cold-heading suitability require separate verification against the product standard, contract and material certificate. ; Table 3, note 2 permits Co≤1.5% to be included in Ni; The existing coupled Ni+Co constraint is retained and is not split into an independent Ni interval.
Combined limits
- Combined-element limits
- Element coefficient
- Nb
- 1
- Ta
- 1
- Requirement
- Combined Nb+Ta 3.15–4.15%
- Lower limit
- 3.15
- Upper limit
- 4.15
- Elements requiring measured values from the same heat
- Nb
- Ta
Verification notes
EN 10095:1999 original Table 3 visually checked row by row; kept distinct from the 2018 German adopted edition.NiCr22Mo9Nb · DIN 17744-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| C | ≤ 0.1 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiCr22Mo9Nb · DIN 17744-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiCr22Mo9Nb · DIN 17750-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiCr22Mo9Nb · DIN 17752-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| C | ≤ 0.1 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Cu | ≤ 0.5 (lower limit not stated) |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiCr22Mo9Nb · GB /T 26030-2010
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| C | ≤ 0.1 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
NiCr22Mo9Nb · ISO 4955-1994
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.4 (lower limit not stated) |
| C | ≤ 0.1 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 20 ~ 23 |
| Fe | ≤ 5 (lower limit not stated) |
| Mn | ≤ 0.5 (lower limit not stated) |
| Mo | 8 ~ 10 |
| Ni | ≥ 58 (upper limit not stated) |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Ti | ≤ 0.4 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.