NHF880
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for NHF880 →NHF880 · Nippon Steel Wire Rods EXE203 2008.3 / Nippon Steel standards (as listed in this catalogue)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Cat. No. EXE203 2008.3 PDF; cover copyright 2008
- Document title
- Nippon Steel Wire Rods
- Table / clause
- Printed page 23, table index 3
- PDF page references
- 13
- Unit
- Mass fraction (%)
- Analysis type
- The original catalogue does not explicitly identify the analysis type for this table
- Manufacturer
- NIPPON STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.13 |
| Si | 0.5 ~ 0.8 |
| Mn | 1.4 ~ 1.7 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Al | 0.01 ~ 0.05 |
| Ti | ≤ 0.2 (lower limit not stated) |
| B | ≥ 0.0005 (upper limit not stated) |
Applicability and limitations
Historical Nippon Steel wire-rod catalogue EXE203 2008.3, PDF page 13
printed page 23, Nippon Steel Standards (as stated in this catalogue). The original catalogue does not explicitly identify the analysis type for this table. Manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: NHF composition follows the original table; Al is not Ar; Mechanical values vary with grade and diameter and are not entered unconditionally in this batch.
Composition conditions
- Original catalogue mass percentages, historical manufacturer data from 2008.3; Referenced standard names and editions follow the original document; this does not establish that the official texts of those standards have been obtained and verified.
- A dash or blank must not be treated as 0; only chemical composition has been checked in this batch. Mechanical properties and actual supply require separate verification under the applicable conditions.
- NHF composition follows the original table; Al is not Ar; Mechanical values vary with grade and diameter and are not entered unconditionally in this batch.