N08020
17 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for N08020 →N08020 · ASTM A240/A240M-2014
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A240/A240M-2014
- Table / clause
- Table 1 and footnotes A–O
- PDF page references
- 1、2、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 32.0 ~ 38.0 |
| Mo | 2.0 ~ 3.0 |
| Cu | 3.0 ~ 4.0 |
| Nb | ≤ 1 (lower limit not stated) |
Applicability and limitations
Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. ; Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. ; This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. ; Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements. ; Other elements in the original table: Cb 8×C min, 1.00 max; See the limits below for the specific coupled requirements.
Combined limits
- Combined-element limits
- Element coefficient
- Nb
- 1
- C
- -8
- Lower limit
- 0
- Upper limit
- Not stated
- Requirement
- Nb≥8×C
- Elements requiring measured values from the same heat
N08020 · ASTM A312/A312M-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A312/A312M-2017
- Table / clause
- Table 1, footnotes A–M and clause 7.1
- PDF page references
- 1、2、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 32.0 ~ 38.0 |
| Mo | 2.0 ~ 3.0 |
| Cu | 3.0 ~ 4.0 |
Applicability and limitations
Table 1, mass percent; A single value is a maximum; ellipses mean unspecified and are not entered as zero. ; Clause 7.1 requires compliance with Table 1; The general A999/A999M requirements in Clause 5.1 still apply; only the chemical-composition table was checked in this batch. ; Austenitic steel pipe standard; This does not directly establish cold-heading wire suitability or compliance with all product acceptance requirements. ; Footnote C: the nitrogen-analysis method is agreed between purchaser and supplier. ; Footnote L gives combined Nb+Ta, with no independent maxima; it is not split into two 1.00% limits.
Combined limits
- Combined-element limits
- Requirement
- Nb+Ta≥8×C
- Element coefficient
- Nb
- 1
- Ta
- 1
- C
- -8
- Lower limit
- 0
- Requirement
- Nb+Ta≤1.00%
- Element coefficient
- Nb
- 1
- Ta
- 1
- Upper limit
- 1
- Elements requiring measured values from the same heat
- Nb
- Ta
N08020 · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Bars
- Original record status
- Manufacturer source verified
- Document edition
- Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
- Document title
- Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
- Table / clause
- Steel grades and chemical composition table
- PDF page references
- 7
- Unit
- Percentages as stated in the original table; refer to the source for the specific basis
- Analysis type
- Analysis type not stated
- Manufacturer
- Walsin Lihwa
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Ni | 32.0 ~ 38.0 |
| Cr | 19.0 ~ 21.0 |
| Mo | 2.0 ~ 3.0 |
| Cu | 3.0 ~ 4.0 |
| Fe | Balance |
Applicability and limitations
Walsin Lihwa official-website catalogue, PDF page 7
printed page 11, row 29; Manufacturer composition table (%), covering billets and bars; analysis type not stated. The official-website filename includes 2024; no edition number is shown inside the document; Not treated as a verified edition of the corresponding standard or a supply guarantee from Creation Group. Condition: Al+Ti=8*C-1; The elements are coupled; no independent Al/Ti value is inserted
Composition conditions
- The original table lists Chemical Composition (%); Heat or product analysis is not identified; the values cannot be treated as guaranteed limits under the corresponding standard.
- The correspondence column gives designation mappings in manufacturer information; No standard year is given, so this is not upgraded to a verified ASTM/GB/JIS/EN/RCC-M standard record.
- Different S, Ni and Ti/Nb conditions for the same grade designation are retained as separate original rows; dashes are not entered as zero.
- Al+Ti=8*C-1; The elements are coupled; no independent Al/Ti value is inserted
Combined limits
- Combined-element limits
- Element coefficient
- Al
- 1
- Ti
- 1
- C
- -8
- Lower limit
- 0
- Element coefficient
- Al
- 1
- Ti
- 1
- Upper limit
- 1
Verification notes
Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.N08020 · ASTM A182/A182M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A182/A182M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A240/240M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A240/240M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A240/A240M-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A276/A276M-2017
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A276/A276M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A479/A479M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A479/A479M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A511/A511M-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A511/A511M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM A959-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM B463-2021
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Special alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N08020 · ASTM B729-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.07 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Cu | 3 ~ 4 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 2 ~ 3 |
| Ni | 32 ~ 38 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.