N07718
6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for N07718 →N07718 · API 6ACRA-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.4 ~ 0.6 |
| B | ≤ 0.006 (lower limit not stated) |
| Bi | ≤ 5e-05 (lower limit not stated) |
| C | ≤ 0.045 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 17 ~ 21 |
| Cu | ≤ 0.23 (lower limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Mo | 2.8 ~ 3.3 |
| Ni | 50 ~ 55 |
| P | ≤ 0.01 (lower limit not stated) |
| Pb | ≤ 0.001 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Se | ≤ 0.0005 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Ti | 0.8 ~ 1.15 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N07718 · API 6ACRA-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.4 ~ 0.6 |
| B | ≤ 0.006 (lower limit not stated) |
| Bi | ≤ 5e-05 (lower limit not stated) |
| C | ≤ 0.045 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 17 ~ 21 |
| Cu | ≤ 0.23 (lower limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Mo | 2.8 ~ 3.3 |
| Ni | 50 ~ 55 |
| P | ≤ 0.01 (lower limit not stated) |
| Pb | ≤ 0.001 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Se | ≤ 0.0005 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Ti | 0.8 ~ 1.15 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N07718 · ASTM B 637-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.2 ~ 0.8 |
| B | ≤ 0.006 (lower limit not stated) |
| C | ≤ 0.08 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 17 ~ 21 |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Mo | 2.8 ~ 3.3 |
| Ni | 50 ~ 55 |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Ti | 0.65 ~ 1.15 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N07718 · ASTM B 637-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.2 ~ 0.8 |
| B | ≤ 0.006 (lower limit not stated) |
| C | ≤ 0.08 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 17 ~ 21 |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Mo | 2.8 ~ 3.3 |
| Nb | 4.75 ~ 5.5 |
| Ni | 50 ~ 55 |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Ti | 0.65 ~ 1.15 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N07718 · ASTM B670-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.2 ~ 0.8 |
| B | ≤ 0.006 (lower limit not stated) |
| C | ≤ 0.08 (lower limit not stated) |
| Co | ≤ 1 (lower limit not stated) |
| Cr | 17 ~ 21 |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Mo | 2.8 ~ 3.3 |
| Ni | 50 ~ 55 |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Ti | 0.65 ~ 1.15 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
N07718 · SAE J467b-1956
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 0.4 ~ 0.4 |
| C | 0.04 ~ 0.04 |
| Cr | 18.6 ~ 18.6 |
| Fe | 18.5 ~ 18.5 |
| Mn | 0.2 ~ 0.2 |
| Mo | 3.1 ~ 3.1 |
| Nb | 5 ~ 5 |
| Si | 0.2 ~ 0.2 |
| Ti | 0.9 ~ 0.9 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.