← BackMaterial grade directory

ML15MN

4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for ML15MN →

ML15Mn · GB/T 5953

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Wire rod
Original record status
Reference transcription of standard
Standard edition
GB/T 6478-2015
Table / clause
Table 3

Carbon-equivalent reference

IIW / CEV:0.3400–0.5333Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2033–0.3133Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2600–0.3850Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.14 ~ 0.2
Si0.1 ~ 0.3
Mn1.2 ~ 1.6
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Clause 6.1.1 of GB/T5953.1/.2:2009 follows the relevant standards identified in the contract; This is reference composition for the same designation under GB/T6478; the applicable standard must be confirmed by contract, and these values are not directly treated as mandatory composition under 5953. No edition is stated on the website; Displayed under this source edition; contract applicability is not established

Verification notes

Standard source: GB/T 6478-2015 · Table 3View associated products →

ML15Mn · GB/T 28906-2025

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Cold-heading steel for quenching and tempering
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 28906-2025
Table / clause
Table 3 · Notes a–d; 7.1.5–7.1.7
PDF page references
8、9、11

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 3 default composition; optional aluminum addition requires agreement
IIW / CEV:0.3200–0.5333Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1833–0.3133Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2400–0.3850Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Table 3, Note a: aluminum may be added to improve cold-heading performance; total Al ≤0.060%
IIW / CEV:0.3200–0.5333Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1833–0.3133Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2400–0.3850Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.12 ~ 0.2
Si0.1 ~ 0.3
Mn1.2 ~ 1.6
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Sn≤ 0.06 (lower limit not stated)

Applicability and limitations

GB/T28906-2025 Table 3: Hot-rolled wire rod of quenching-and-tempering-type cold-heading steel; heat analysis, mass fraction %.. ; Note a: Aluminum may be added to improve cold-heading performance, with Alt≤0.060%; this option does not make addition mandatory by default.. ; Note b: Through negotiation between the supplier and the buyer, Si may be lower than 0.10%; In this case, aluminum must be added and Alt≥0.020%.. This record defaults to the Si range listed in the table; do not arbitrarily fill in when no specific low-silicon agreement range is given. ; Note c: For the first 11 grades in Table 3, Cr may be added by agreement to improve hardenability and mechanical properties; the addition amount must be confirmed by both parties; When no agreement is provided, residual Cr ≤ 0.20% according to 7.1.5. ; 7.1.5 Residual Cr, Ni, and Cu are each ≤ 0.20%, and residual Sn ≤ 0.06%; The residual Cr upper limit is not applicable when Cr has a listed alloy range in the table. ; 7.1.7 Unless otherwise specified in the table, the permissible deviation of the finished product chemical composition shall be according to GB/T222; heat analysis values shall not be substituted for finished product tolerances. ; The original text applies to 5–52mm hot-rolled wire rod for cold heading; specific product specifications, supply, and processing routes still need to be confirmed; Mechanical properties to be verified separately.

Original condition-branch records

Table 3 default composition; optional aluminum addition requires agreement

ElementComposition requirement
C0.12 ~ 0.2
Si0.1 ~ 0.3
Mn1.2 ~ 1.6
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Sn≤ 0.06 (lower limit not stated)

Table 3, Note a: aluminum may be added to improve cold-heading performance; total Al ≤0.060%

ElementComposition requirement
C0.12 ~ 0.2
Si0.1 ~ 0.3
Mn1.2 ~ 1.6
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Sn≤ 0.06 (lower limit not stated)
Al≤ 0.06 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Original PDF pp. 8–9, Table 3, and residual-element clause on p. 11 visually checked

ML15Mn · GB/T 6478-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Cold-heading steel for quenching and tempering
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 6478-2015
Table / clause
Table 3; 6.1.5–6.1.7
PDF page references
9、10

Carbon-equivalent reference

IIW / CEV:0.3400–0.5333Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2033–0.3133Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2600–0.3850Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.14 ~ 0.2
Si0.1 ~ 0.3
Mn1.2 ~ 1.6
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Table 3: Heat analysis of quenching-and-tempering-type steels for cold heading and cold extrusion; mass fraction %.. ; 6.1.5 Residual Cr/Ni/Cu each ≤0.20%; the residual Cr limit shall not be used when an alloy Cr range is specified. ; 6.1.7 Permissible deviations of finished product composition shall be in accordance with GB/T222; This record does not widen the default heat-analysis limits by applying product-analysis tolerances.. ; Table 3 of this edition does not specify optional Al or a unified low Si agreement; conditions of GB28906-2025 shall not be applied. ; Unspecified elements such as Mo shall not be assumed zero; Specific product forms, delivery, mechanical properties, and applicability to part forming still require separate verification.

Verification notes

Original PDF9, Table 3 and PDF10 residual-content provisions were visually checked

ML15Mn · GB/T 6478-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 6478-2001
Table / clause
Table 3 / 6.1.4–6.1.8
PDF page references
5、6

Carbon-equivalent reference

IIW / CEV:0.3400–0.5333Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2067–0.3167Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2600–0.3850Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.14 ~ 0.2
Si0.2 ~ 0.4
Mn1.2 ~ 1.6
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)

Applicability and limitations

GB/T6478-2001, Table 3, heat analysis wt%; 6.1.4 residual Cr/Ni/Cu are each ≤.20%; alloy Cr ranges are not subject to the residual maximum. ; 6.1.8 product-analysis tolerances require separate verification under GB/T222-1984, Table 2, and do not widen the default heat-analysis range. ; Actual 2001 edition; Composition from editions 2015 or 2025 is not substituted for this edition; specific dimensions and delivery mechanical properties require separate verification.

Verification notes

Visual check of four composition tables and clauses on pages 5 and 6 of the original PDF
WhatsApp Technical enquiry →