← BackMaterial grade directory

ML06CR17NI12MO2

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for ML06CR17NI12MO2 →

ML06Cr17Ni12Mo2 · GB /T 4232-2019

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
GB/T 4232-2009
Table / clause
Table 1 categories/delivery conditions, Table 2 heat composition and Clause 6/7.1
PDF page references
1、5、6、7、8

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

The chemical composition currently shown is transcribed from the original GB/T 4232-2009; The original record cites GB /T 4232-2019; that original edition remains unavailable, and differences between editions have not been confirmed. GB/T4232—2009 "Stainless steel wire for cold heading", Table 1/2 and 7.1, heat analysis wt%. ; In this edition of Table 2, values for which no range is specified are all maximum values; Blanks are not entered as zero. ; ML06Cr12Ti/ML06Cr12Nb respectively require Ti/Nb to satisfy ≥6C and ≤1.00%; check the coupled limits.. ; Soft condition S: nominal diameter .80–11.0mm; lightly drawn condition LD: .80–20.0mm.; Delivery condition and mechanical conditions must be selected and verified separately. ; Apply product-analysis composition tolerances under GB/T222 separately; do not incorporate them into the heat-analysis values in Table 2.. ; The standard is explicitly for cold upsetting; The company's actual scope of supply, performance, and quality assurance still require confirmation via product documentation.. ; The 2009 edition is actually adopted, which does not indicate that the 2019 edition composition has been verified; ML06Cr18Ni11Ti shall not be associated with other grades in this table based on approximate names.

Verification notes

The chemical composition currently shown is transcribed from the original GB/T 4232-2009; The original record cites GB /T 4232-2019; that original edition remains unavailable, and differences between editions have not been confirmed.

ML06Cr17Ni12Mo2 · GB/T 4232-2009

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Wire
Original record status
Original standard verified
Standard edition
GB/T 4232-2009
Table / clause
Table 1 categories/delivery conditions, Table 2 heat composition and Clause 6/7.1
PDF page references
1、5、6、7、8

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

GB/T4232—2009 "Stainless steel wire for cold heading", Table 1/2 and 7.1, heat analysis wt%. ; In this edition of Table 2, values for which no range is specified are all maximum values; Blanks are not entered as zero. ; ML06Cr12Ti/ML06Cr12Nb respectively require Ti/Nb to satisfy ≥6C and ≤1.00%; check the coupled limits.. ; Soft condition S: nominal diameter .80–11.0mm; lightly drawn condition LD: .80–20.0mm.; Delivery condition and mechanical conditions must be selected and verified separately. ; Apply product-analysis composition tolerances under GB/T222 separately; do not incorporate them into the heat-analysis values in Table 2.. ; The standard is explicitly for cold upsetting; The company's actual scope of supply, performance, and quality assurance still require confirmation via product documentation.. ; The 2009 edition is actually adopted, which does not indicate that the 2019 edition composition has been verified; ML06Cr18Ni11Ti shall not be associated with other grades in this table based on approximate names.

Verification notes

Table 1/2 and applicable provisions of the official national standard were visually checked
WhatsApp Technical enquiry →