MFT10
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for MFT10 →MFT10 · GB/T 28906-2025
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Cold-heading steel not intended for quenching and tempering
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 28906-2025
- Table / clause
- Table 5 · Footnotes; 7.1.5–7.1.7
- PDF page references
- 7、11
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.2 ~ 0.28 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 1.2 ~ 1.6 |
| Nb | ≤ 0.08 (lower limit not stated) |
| V | 0.03 ~ 0.08 |
| Cr | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Sn | ≤ 0.06 (lower limit not stated) |
Applicability and limitations
Mass percent, heat analysis, GB/T28906-2025 Table 5. ; 7.1.5 residual Cr/Ni/Cu are each ≤0.20% and Sn≤0.06%; tabulated alloy Cr is not subject to the residual maximum; 7.1.7 product-analysis tolerances follow GB/T222 and must not be directly treated as heat-analysis limits. ; The standard scope for hot-rolled cold-heading wire rod does not replace confirmation of actual supply dimensions and the component manufacturing process; Mechanical properties require separate verification. ; Table 5 Note a: Mo/Ti/B/Al/N and other elements may be added by agreement between both parties according to strength and product-size requirements, with the agreement stated in the contract; do not fill in values where no uniform range is given. ; B at the end of MFT grades indicates a ferrite + bainite structure and does not represent a specified boron content; Do not enter 0 if B is not specified.
Verification notes
Visual check of the original composition table and footnotesMFT10 · GB/T 6478-2015
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Subcategory
- Cold-heading steel not intended for quenching and tempering
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 6478-2015
- Table / clause
- Table 5 · Footnotes; 6.1.5–6.1.7
- PDF page references
- 10
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.14 |
| Si | 0.2 ~ 0.35 |
| Mn | 1.9 ~ 2.3 |
| Nb | ≤ 0.2 (lower limit not stated) |
| V | ≤ 0.1 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
GB/T6478-2015, Table 5, heat-analysis mass percentages. ; 6.1.5 residual Cr/Ni/Cu are each ≤.20%; tabulated alloy Cr is not subject to the residual Cr maximum. ; 6.1.7 product-analysis tolerances follow GB/T222 and do not widen the default heat-analysis range; Where Sn is unspecified, limits from a newer edition are not inserted. ; Specific dimensions, product condition and mechanical-property conditions require separate verification; composition alone does not establish suitability for forming a component. ; Table 5 permits additions such as Cr/B according to strength and size requirements; no general range is given and B is not inserted without a source; The default Cr limit is a residual-content requirement.
Verification notes
Visual check of all relevant ranges and footnotes in original Tables 1, 2, 4 and 5MFT10 · GB/T 29087-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Subcategory
- Cold-heading steel not intended for quenching and tempering
- Material form
- Hot-rolled non-quenched-and-tempered cold-heading steel wire rod; delivered in the hot-rolled condition
- Original record status
- Original standard verified
- Standard edition
- GB/T 29087-2012
- Table / clause
- Table 1 · Notes 1, 2; 6.1.1–6.1.2
- PDF page references
- 1、7、8
- Unit
- Mass fraction (%)
- Analysis type
- Heat analysis
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.14 |
| Si | 0.2 ~ 0.35 |
| Mn | 1.9 ~ 2.3 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Nb | ≤ 0.2 (lower limit not stated) |
| V | ≤ 0.1 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| N | ≤ 0.008 (lower limit not stated) |
Applicability and limitations
GB/T 29087-2012 Table 1 heat analysis mass fraction %, Table 1 lists only three grades: MFT8, MFT9, and MFT10. ; Table 1 Note: Other elements such as Cr and B may be added according to strength level and specification; no unified limits are provided, and these shall not be treated as default composition ranges. ; Table 1 Note: Ni and Cu are residual elements each ≤0.20%, N ≤0.008%; Product permissible deviations shall be verified separately according to GB/T 222. ; This standard specifies hot-rolled wire rod of non-quenched-and-tempered cold heading steel, delivered in the hot-rolled condition; Mechanical properties in Table 2 and cold upsetting conditions in 6.6 shall be verified in conjunction with specifications and contracts. ; Compositions of grades with the same name in versions such as GB/T 6478-2015 and GB/T 28906-2025 shall not be automatically interchangeable.