Open condition selection, comparison and carbon-equivalent tools for KTCH10AT →KTCH10AT · Kobe Steel manufacturer specification (section 6-9)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Cold-heading wire rod for extended die life
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-9
- PDF page references
- 31
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.13 |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | 0.3 ~ 0.6 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Al | ≥ 0.02 (upper limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Original composition for cold-heading wire rod intended to extend tool life in the Kobe Steel catalogue, section 6-9 (PDF page 31), mass fractions wt%; This is not the original JIS/SAE standard. The catalogue does not state a publication year; supply and process applicability require separate confirmation.
Composition conditions
- Original-table mass percentage, Section 6-9; Dashes and unlisted elements are not entered as zero.
- The original Cr entry is addition, indicating qualitative addition only, without a numerical range.
- The original B entry is addition, indicating qualitative addition only, without a numerical range.
- Common footnote to the two tables in 6-9: Cu≤0.30%, Ni≤0.20%, Cr≤0.20%; Cr “Addition” indicates only the intention to add.
- The manufacturer catalogue does not identify the publication edition; Catalogue information does not establish current supply dimensions.