Open condition selection, comparison and carbon-equivalent tools for KNCH8S →KNCH8S · Kobe Steel manufacturer specification (section 6-7)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Wire rod for bolts produced without quenching and tempering
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-7
- PDF page references
- 27
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.27 ~ 0.33 |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | 1.35 ~ 1.65 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Original composition for wire rod for bolts made without quenching and tempering in the Kobe Steel catalogue, section 6-7 (PDF page 27), mass fractions wt%; This is not the original JIS/SAE standard. The catalogue does not state a publication year; supply and process applicability require separate confirmation.
Composition conditions
- Original-table mass percentage, Section 6-7; Dashes and unlisted elements are not entered as zero.
- The original Cr entry is addition, indicating qualitative addition only, without a numerical range.
- Footnote below Table 6-7: P/S≤0.030%, Cu≤0.30%, Ni≤0.20%.