KMN36-A

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for KMN36-A →

KMN36-A · Kobe Steel manufacturer specification (section 6-12)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Manganese steel for mechanical structures
Material form
Bars
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-12
PDF page references
31
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.5500–0.6767 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3800–0.4667 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4500–0.5500 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.3 ~ 0.36
Si0.15 ~ 0.35
Mn1.5 ~ 1.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Original composition for manganese steel for machine structures in the Kobe Steel catalogue, section 6-12 (PDF page 31), mass fractions wt%; This is not the original JIS/SAE standard. The catalogue does not state a publication year; supply and process applicability require separate confirmation.

Composition conditions

Verification notes

The original manufacturer table was checked cell by cell against the PDF table; Qualitative Addition has no numerical lower or upper limit.