KKG4 · Kobe Steel manufacturer specification (section 6-20)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Gear steel
Material form
Bars
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-20
PDF page references
36
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.5017–0.7567Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2633–0.3917Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3025–0.4487 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si≤ 0.15 (lower limit not stated)
Mn0.55 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.85 ~ 1.25
Mo0.35 ~ 0.45

Applicability and limitations

Original composition for gear steel in the Kobe Steel catalogue, section 6-20 (PDF page 36), mass fractions wt%; This is not the original JIS/SAE standard. Actual supply and process applicability require separate confirmation.

Composition conditions

Verification notes

Chemical values checked cell by cell against the manufacturer original table; columns joined during extraction in Section 6-17 were additionally checked manually against the original image.