← BackMaterial grade directory

KCH6AT

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for KCH6AT →

KCH6AT · Kobe Steel manufacturer specifications (KCH series)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-8-A · KCH A · aluminium-killed · series
PDF page references
29
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.0417–0.2200Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0125–0.1317Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0250–0.1500Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
Mn0.25 ~ 0.4
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
Cu≤ 0.3 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)

Applicability and limitations

Kobe Steel manufacturer KCH A · aluminium-killed · series, original table composition (PDF page 29), mass fraction wt%; not the original JIS/AISI standards. Equivalent or similar grades are catalogue references only and do not guarantee direct substitution or current supply by Creation Group.

Composition conditions

Verification notes

Manufacturer original table extracted cell by cell from the PDF; page images used to check headers and the shared Cu/Ni/Cr footnote.
WhatsApp Technical enquiry →