KCH35AT
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for KCH35AT →KCH35AT · Kobe Steel manufacturer specifications (KCH series)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-8-A · KCH A · aluminium-killed · series
- PDF page references
- 29
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.32 ~ 0.38 |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Al | ≥ 0.02 (upper limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Kobe Steel manufacturer KCH A · aluminium-killed · series, original table composition (PDF page 29), mass fraction wt%; not the original JIS/AISI standards. Equivalent or similar grades are catalogue references only and do not guarantee direct substitution or current supply by Creation Group.
Composition conditions
- Original table for the aluminium-killed KCH A series in mass percent; dashes and unlisted elements are not filled with zero.
- Table note: Cu≤0.30%, Ni≤0.20%, Cr≤0.20%.
- The manufacturer catalogue does not identify the publication edition; Catalogue information does not establish current supply dimensions.