KCH33KT
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for KCH33KT →KCH33KT · Kobe Steel manufacturer specifications (KCH series)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Wire rod
- Composition basis
- Manufacturer-published composition range
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-8 · KCH xx K · series
- PDF page references
- 28
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.31 ~ 0.36 |
| Si | 0.15 ~ 0.3 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Kobe Steel manufacturer specifications for carbon-steel wire rod for cold heading, not the original JIS or AISI standards. Similar standard grades in the catalogue do not establish direct substitutability or supply by our company. Publication edition not stated.
Composition conditions
- Table note: Cu≤0.30%, Ni≤0.20%, Cr≤0.20%; chemistry is in mass percent.
- The catalogue gives no publication edition; file creation time is not treated as the technical specification's effective year.