← BackMaterial grade directory

HSN72-1

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HSN72-1 →

HSn72-1 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 36, designation C44300
PDF page references
8、9

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Products other than tube, base composition in Table 3
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Tubular products: Table 3, note d raises the Sn minimum to 0.9%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
Cu70.0 ~ 73.0
As0.02 ~ 0.06
Sn0.8 ~ 1.2
Fe≤ 0.06 (lower limit not stated)
Pb≤ 0.07 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 36, designation C44300. Zn is the balance; Unlisted elements are not entered as zero; Sum of impurities listed in table ≤0.4%, calculated according to Clause 2.3 and footnotes. Table 3 Note d: When this grade is a tube product, the minimum mass fraction of Sn is 0.9%; For other products, the tabulated lower limit of 0.8% applies..

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Original condition-branch records

      Products other than tube, base composition in Table 3

      ElementComposition requirement
      Cu70.0 ~ 73.0
      As0.02 ~ 0.06
      Sn0.8 ~ 1.2
      Fe≤ 0.06 (lower limit not stated)
      Pb≤ 0.07 (lower limit not stated)

      Tubular products: Table 3, note d raises the Sn minimum to 0.9%

      ElementComposition requirement
      Cu70.0 ~ 73.0
      As0.02 ~ 0.06
      Sn0.9 ~ 1.2
      Fe≤ 0.06 (lower limit not stated)
      Pb≤ 0.07 (lower limit not stated)

      A condition branch must be selected

      Yes

      Verification notes

      Each cell in row 36 of Table 3 in the scanned original, together with applicable footnotes, was checked manually
      WhatsApp Technical enquiry →