← BackMaterial grade directory

HPB89-2

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HPB89-2 →

HPb89-2 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 2 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 2 standard condition
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Table 2, Note 1: Fe ≤0.030% for non-magnetic brass; do not automatically combine with other purchasing conditions
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
Fe≤ 0.1 (lower limit not stated)
Pb1.3 ~ 2.5
Ni≤ 0.7 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Zn is the balance; Total impurities exclude elements specified as alloying constituents; all listed elements must not simply be added together. Corresponding foreign grade designation shown in the original table: C31400; Note 4 includes Ni, other than the principal constituents, in Cu, subject to the combined Cu+Ni limit; This does not establish automatic substitution across standards. Note 5/6/7 requires Cu and the listed elements to total ≥99.6%; This includes a balance element; independent limits cannot be used to derive a guaranteed range. Table 2, note 1: Fe≤0.030% applies to nonmagnetic brass only where nonmagnetic performance is expressly required; Ordinary conditions are not automatically tightened.

Combined limits

Combined-element limits
  • Element coefficient
    Cu
    1
    Ni
    1
    Lower limit
    87.5
    Upper limit
    90.5
    Requirement
    For the corresponding foreign-grade row, Ni is included in Cu under note 4
Elements requiring measured values from the same heat
  • Cu

Original condition-branch records

Table 2 standard condition

ElementComposition requirement
Fe≤ 0.1 (lower limit not stated)
Pb1.3 ~ 2.5
Ni≤ 0.7 (lower limit not stated)

Table 2, Note 1: Fe ≤0.030% for non-magnetic brass; do not automatically combine with other purchasing conditions

ElementComposition requirement
Fe≤ 0.03 (lower limit not stated)
Pb1.3 ~ 2.5
Ni≤ 0.7 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.

HPb89-2 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 16, designation C31400
PDF page references
7、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu87.5 ~ 90.5
Fe≤ 0.1 (lower limit not stated)
Pb1.3 ~ 2.5
Ni≤ 0.7 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 16, designation C31400. Zn is balance. Total table-listed impurities ≤1.2%; confirm the calculation scope under clause 2.3 and the row footnotes. A partial sum of listed elements does not replace complete analysis. Note a to Table 3: Fe≤0.030% for nonmagnetic brass applies only to that condition, not to this leaded-brass row. Clause 2.2: unlisted elements are not assigned zero. Clause 2.4: balance Zn must not be mechanically converted into a guaranteed range.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Each cell in row 16 of Table 3 in the scanned original, together with applicable footnotes, was checked manually