← BackMaterial grade directory

HPB59-2

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HPB59-2 →

HPb59-2 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 30, designation T38200
PDF page references
7、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu57.0 ~ 60.0
Fe≤ 0.5 (lower limit not stated)
Pb1.5 ~ 2.5
Sn≤ 0.5 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 30, designation T38200. Zn is the balance; Tabulated total impurities ≤1.0%; The calculation scope must be confirmed under Clause 2.3 and the footnotes for this row; a partial sum of listed elements cannot replace complete analysis. Table 3, note a: nonmagnetic-brass condition Fe≤0.030% applies only to nonmagnetic brass and is not applied to this leaded-brass row. Clause 2.2: unlisted elements are not entered as zero; Clause 2.4: the Zn balance must not be mechanically converted into a guaranteed range. Table 3, note c: total impurities for this row are the sum of measured contents of the impurity elements listed in the table.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Each cell in row 30 of Table 3 in the scanned original, together with applicable footnotes, was checked manually
      WhatsApp Technical enquiry →