1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for HMN64-8-5-1.5 →HMn64-8-5-1.5 · GB/T 5231-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 3, row 51, designation T67100
- PDF page references
- 8、9
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cu | 63.0 ~ 66.0 |
| Al | 4.5 ~ 6.0 |
| Si | 1.0 ~ 2.0 |
| Sn | ≤ 0.5 (lower limit not stated) |
| Ni | ≤ 0.5 (lower limit not stated) |
| Mn | 7.0 ~ 8.0 |
| Fe | 0.5 ~ 1.5 |
| Pb | 0.3 ~ 0.8 |
Applicability and limitations
Mass fraction wt%; GB/T5231—2012, Table 3, row 51, designation T67100. Zn is the balance; A dash means unspecified; it is not entered as zero. Tabulated total impurities ≤1.0%, evaluated under Clause 2.3; a partial sum of listed values cannot replace complete analysis.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat