HMN57-2-2-0.5

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HMN57-2-2-0.5 →

HMn57-2-2-0.5 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 59, designation T67420
PDF page references
9
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu56.5 ~ 58.5
Fe0.3 ~ 0.8
Pb0.3 ~ 0.8
Al1.3 ~ 2.1
Mn1.5 ~ 2.3
Ni≤ 0.5 (lower limit not stated)
Si0.5 ~ 0.7
Sn≤ 0.5 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 3, row 59, designation T67420; scanned PDF, PDF physical page 9. Zn is balance; dashes mean unspecified and are not replaced with zero. Clause 2.2: single impurity values in the table are maxima. The total of table-listed impurities is ≤1% and must be checked against measured values for the impurity elements specified in the standard. This standard provides the grade-composition basis for wrought copper and copper alloys; actual supply and cold-heading suitability require separate confirmation.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      The original scanned standard, Table 3 was manually checked cell by cell; Coupled elements and application-specific footnotes require separate verification