HBI60-1.3
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for HBI60-1.3 →HBi60-1.3 · GB/T 5231-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 3, row 44, designation T49240
- PDF page references
- 8
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cu | 58.0 ~ 62.0 |
| Bi | 0.3 ~ 2.3 |
| Cd | ≤ 0.01 (lower limit not stated) |
| Fe | ≤ 0.1 (lower limit not stated) |
| Pb | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Mass fraction wt%; GB/T5231—2012, Table 3, row 44, designation T49240. Zn is the balance; A dash means unspecified; it is not entered as zero; Tabulated total impurities ≤0.3%. Table 3, note c: total impurities are the sum of measured contents of the impurity elements listed in the table; The principal alloying constituent Bi must not be counted as an impurity. Table 3 Note e: 0.05%~1.2% in column Sn is the combined range of Sb+B+Ni+Sn, and cannot be treated as the range of a single element Sn; These four items shall be summed based on actual analysis.
Combined limits
- Combined-element limits
- Requirement
- Table 3, note e: combined Sb+B+Ni+Sn
- Element coefficient
- Sb
- 1
- B
- 1
- Ni
- 1
- Sn
- 1
- Lower limit
- 0.05
- Upper limit
- 1.2
- Elements requiring measured values from the same heat
- Sb
- B
- Ni
- Sn