HBI60-1.0-0.05

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HBI60-1.0-0.05 →

HBi60-1.0-0.05 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 45, designation C49260
PDF page references
8
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu58.0 ~ 63.0
Si≤ 0.1 (lower limit not stated)
Bi0.5 ~ 1.8
Cd≤ 0.001 (lower limit not stated)
Sn≤ 0.5 (lower limit not stated)
P0.05 ~ 0.15
Fe≤ 0.5 (lower limit not stated)
Pb≤ 0.09 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 45, designation C49260. Zn is the balance; A dash means unspecified; it is not entered as zero; Tabulated total impurities ≤1.5%.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Scanned original: Table 3, row 45 and note c/e checked cell by cell