HASTELLOY G-30
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for HASTELLOY G-30 →Hastelloy G-30 · Alloy Wire International manufacturer catalogue (edition not stated)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Wire
- Composition basis
- Manufacturer typical composition range
- Original record status
- Manufacturer source verified
- Document edition
- The original text does not specify the publication version; PDF metadata 2015-07-22 only records the generation date
- Document title
- AWBrochure manufacturer product catalogue
- Table / clause
- Approximate chemical composition
- PDF page references
- 26
- Unit
- Percentages as stated in the original table; refer to the source for the specific basis
- Analysis type
- Manufacturer approximate composition, not measured heat or product analysis
- Manufacturer
- Alloy Wire International
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| Ni | Typical/nominal value 43.0 (not a guaranteed range) |
| Cr | 28.0 ~ 31.5 |
| Fe | 13.0 ~ 17.0 |
| Mo | 4.0 ~ 6.0 |
| Co | ≤ 5.0 (lower limit not stated) |
| W | 1.5 ~ 4.0 |
Applicability and limitations
Alloy Wire International original catalogue, PDF page 26
printed page 25. Original publication edition not stated; metadata 2015-07-22 is not an edition. Approximate chemical composition: manufacturer approximate composition, single values are approximate, BAL means balance. Neither standard guaranteed values nor measured heat analysis; does not establish supply by our company. Display only; excluded from standard-limit reverse search.
Composition conditions
- The original text explicitly labels the entire column as APPROXIMATE CHEMICAL COMPOSITION, not delivery guarantee limits.
- Single values shall be saved as nominal and marked as approximate values; do not set min=max; BAL shall not be calculated as a number or treated as 0; Shall not be used for standard limit reverse-lookup.
- IIW/Pcm/CET are not applied to this batch of nickel-based/high-alloy/stainless/copper/titanium materials; Material application and manufacturer supply capability still require verification.