HASTELLOY B-2

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for HASTELLOY B-2 →

Hastelloy B-2 · Alloy Wire International manufacturer catalogue (edition not stated)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Nickel and nickel alloys
Subcategory
Nickel and nickel alloys
Material form
Wire
Composition basis
Manufacturer typical composition range
Original record status
Manufacturer source verified
Document edition
The original text does not specify the publication version; PDF metadata 2015-07-22 only records the generation date
Document title
AWBrochure manufacturer product catalogue
Table / clause
Approximate chemical composition
PDF page references
20
Unit
Percentages as stated in the original table; refer to the source for the specific basis
Analysis type
Manufacturer approximate composition, not measured heat or product analysis
Manufacturer
Alloy Wire International

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
NiTypical/nominal value 69.0 (not a guaranteed range)
MoTypical/nominal value 28.0 (not a guaranteed range)
Fe≤ 2.0 (lower limit not stated)
Cr≤ 1.0 (lower limit not stated)
Co≤ 1.0 (lower limit not stated)

Applicability and limitations

Alloy Wire International original catalogue, PDF page 20

printed page 19. Original publication edition not stated; metadata 2015-07-22 is not an edition. Approximate chemical composition: manufacturer approximate composition, single values are approximate, BAL means balance. Neither standard guaranteed values nor measured heat analysis; does not establish supply by our company. Display only; excluded from standard-limit reverse search.

Composition conditions

Verification notes

All 47 grade compositions were checked against original images; nominal values, one-sided limits, ranges, BAL balance and totals remain separate.