- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 3, row 13, designation T23030
- PDF page references
- 7、9
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cu | 84 ~ 86 |
| Fe | ≤ 0.1 (lower limit not stated) |
| Pb | ≤ 0.03 (lower limit not stated) |
| As | 0.02 ~ 0.08 |
Applicability and limitations
Mass fraction wt%; GB/T5231—2012, Table 3, row 13, designation T23030. Zn is the balance; A dash means unspecified; it is not entered as zero. Clause 2.2: single values for other impurity elements are maxima. Tabulated total impurities ≤0.3%, evaluated under Clause 2.3; a partial sum of listed values cannot replace complete analysis.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat