HAs68-0.04 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 15, designation T26330
PDF page references
7、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu67 ~ 70
Fe≤ 0.1 (lower limit not stated)
Pb≤ 0.03 (lower limit not stated)
As0.03 ~ 0.06

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 15, designation T26330. Zn is the balance; A dash means unspecified; it is not entered as zero. Clause 2.2: single values for other impurity elements are maxima. Tabulated total impurities ≤0.3%, evaluated under Clause 2.3; a partial sum of listed values cannot replace complete analysis.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Each cell in row 15 of Table 3 in the scanned original, together with applicable footnotes, was checked manually
      WhatsApp Technical enquiry →