← BackMaterial grade directory

H95

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for H95 →

H95 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 3, row 1, designation C21000
PDF page references
7、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu94 ~ 96
Fe≤ 0.05 (lower limit not stated)
Pb≤ 0.05 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T5231—2012, Table 3, row 1, designation C21000. Zn is balance. Total table-listed impurities ≤0.3%, covering all impurities outside the principal constituents. A partial sum of listed elements does not replace complete impurity analysis. Clause 2.2: single values for other impurity elements are maxima; unlisted limits require purchaser-supplier agreement and are not replaced with zero. This standard covers wrought copper/copper-alloy designations and chemical composition only; it does not establish actual cold-heading wire supply.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Each cell in row 1 of Table 3 in the scanned original, together with applicable footnotes, was checked manually