GSWRCH38K-B
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for GSWRCH38K-B →GSWRCH38K-B · Xingtai Steel high-end cold-heading steel wire rod (filename marked 244-2019; document number in the body pending verification)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified; edition not confirmed
- Standard edition
- Filename marked 244-2019; document number in the body pending verification
- Table / clause
- Table 1, row 95
- PDF page references
- 3
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.35 ~ 0.41 |
| Si | 0.1 ~ 0.35 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Mass fraction wt%; Manufacturer document, Table 1, heat analysis; PDF, page 3. The PDF main text lacks a cover and shows no standard number; The filename states “244—2019”; PDF was created in 2019, and this designation is not treated as a verified standard edition. G denotes Xingtai Steel high-end wire rod; -A/-B/-C is a quality-class suffix and must not be treated as boron B or aluminum-killed A. Check product-analysis tolerances under GB/T 222; This table gives heat-analysis ranges and must not be directly treated as guaranteed product-analysis ranges. This record does not establish Creation Group stock availability, customer approval or direct substitution. Table 1, merged residual-element cell: each Cr/Ni/Cu ≤0.20%. Clause 5.4: for high or relatively high cold-upsetting requirements, specimens with C at least 0.30% or containing alloying elements must first be spheroidize-annealed as specified in the clause; A range crossing the threshold requires assessment against the actual heat and contract.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat