GSWRCH12K-A

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for GSWRCH12K-A →

GSWRCH12K-A · Xingtai Steel high-end cold-heading steel wire rod (filename marked 244-2019; document number in the body pending verification)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Material form
Wire rod
Original record status
Manufacturer source verified; edition not confirmed
Standard edition
Filename marked 244-2019; document number in the body pending verification
Table / clause
Table 1, row 42
PDF page references
2
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV:0.1500–0.3167Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1183–0.2150Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1300–0.2350Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.1 ~ 0.15
Si0.1 ~ 0.35
Mn0.3 ~ 0.6
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; manufacturer file, Table 1 ladle analysis; PDF p. 2. The PDF body has no cover and no standard number was found; the filename says “244—2019” and the PDF was created in 2019, which does not establish a verified standard edition. G denotes Xingtai Steel high-grade wire rod; suffixes -A/-B/-C are quality grades, not boron B or aluminium-killed A. Product-analysis tolerances are checked under GB/T 222; this table is a ladle range, not directly a guaranteed product range. This record does not represent our stock, customer approval or direct substitutability. Table 1 residual-element merged cells: Cr/Ni/Cu each ≤0.20%.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Xingtai Steel G-series PDF, Table 1, page 2: checked row by row, including merged cells; no basis for a standard number was found in the document body.