GRADE 660
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for GRADE 660 →Grade 660 · ASTM A 453/453M-2002
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.35 (lower limit not stated) |
| B | 0.001 ~ 0.01 |
| C | ≤ 0.08 (lower limit not stated) |
| Cr | 13.5 ~ 16 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 1 ~ 1.5 |
| Ni | 24 ~ 27 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| Ti | 1.9 ~ 2.35 |
| V | 0.1 ~ 0.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
Grade 660 · ASTM A453/453M-2017
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Precipitation-hardening stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.35 (lower limit not stated) |
| B | 0.001 ~ 0.01 |
| C | ≤ 0.08 (lower limit not stated) |
| Cr | 13.5 ~ 16 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 1 ~ 1.5 |
| Ni | 24 ~ 27 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| Ti | 1.9 ~ 2.35 |
| V | 0.1 ~ 0.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
Grade 660 · ASTM A453/453M-2026
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Precipitation-hardening stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.35 (lower limit not stated) |
| B | 0.001 ~ 0.01 |
| C | ≤ 0.08 (lower limit not stated) |
| Cr | 13.5 ~ 16 |
| Mn | ≤ 2 (lower limit not stated) |
| Mo | 1 ~ 1.5 |
| Ni | 24 ~ 27 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| Ti | 1.9 ~ 2.35 |
| V | 0.1 ~ 0.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.