GML40CR

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for GML40CR →

GML40Cr · Xingtai Steel high-end cold-heading steel wire rod (filename marked 244-2019; document number in the body pending verification)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Material form
Wire rod
Original record status
Manufacturer source verified; edition not confirmed
Standard edition
Filename marked 244-2019; document number in the body pending verification
Table / clause
Table 4, row 5
PDF page references
5
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV:0.6600–0.8500Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4550–0.5733Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4850–0.6050Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.38 ~ 0.45
Si≤ 0.3 (lower limit not stated)
Mn0.6 ~ 0.8
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cr0.9 ~ 1.2
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Manufacturer document, Table 4, heat analysis; PDF, page 5. The PDF main text lacks a cover and shows no standard number; The filename states “244—2019”; PDF was created in 2019, and this designation is not treated as a verified standard edition. G denotes Xingtai Steel high-end wire rod; -A/-B/-C is a quality-class suffix and must not be treated as boron B or aluminum-killed A. Check product-analysis tolerances under GB/T 222; This table gives heat-analysis ranges and must not be directly treated as guaranteed product-analysis ranges. This record does not establish Creation Group stock availability, customer approval or direct substitution. Table 4: Al unspecified, residual Ni/Cu are each ≤0.20%. Clause 5.4: for high or relatively high cold-upsetting requirements, specimens with C at least 0.30% or containing alloying elements must first be spheroidize-annealed as specified in the clause; A range crossing the threshold requires assessment against the actual heat and contract.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Xingtai Steel G-series PDF, Table 4, page 5: checked row by row, including merged cells; no basis for a standard number was found in the document body.