← BackMaterial grade directory

GH2132

8 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for GH2132 →

GH2132 · GB /T 14992-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Mn1 ~ 2
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.75 ~ 2.35
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GB /T 14994-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Mn1 ~ 2
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.8 ~ 2.35
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GB /T 14995-2010

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.003 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Cu≤ 0.25 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.75 ~ 2.3
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GB /T 14996-2010

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.003 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Cu≤ 0.25 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.75 ~ 2.3
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GB /T 40313-2021

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Cu≤ 0.25 (lower limit not stated)
Mn1 ~ 2
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.03 (lower limit not stated)
S≤ 0.008 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.8 ~ 2.35
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GJB 2611A-2006

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.35 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Mn≤ 2 (lower limit not stated)
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.9 ~ 2.35
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · GJB 3167-1988

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Mn1 ~ 2
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si0.4 ~ 1
Ti1.75 ~ 2.35
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

GH2132 · YB /T 5245-1993

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.4 (lower limit not stated)
B0.001 ~ 0.01
C≤ 0.08 (lower limit not stated)
Cr13.5 ~ 16
Cu≤ 0.25 (lower limit not stated)
Mn1 ~ 2
Mo1 ~ 1.5
Ni24 ~ 27
P≤ 0.02 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Ti1.75 ~ 2.3
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →