G12144

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for G12144 →

G12144 · ASTM A29/A29M-2012

Original-source verification is incomplete; this is not a formal standard reference

Material category
Spring steels
Subcategory
Spring steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.85 ~ 1.15
P0.04 ~ 0.09
Pb0.15 ~ 0.35
S0.26 ~ 0.35

Applicability and limitations

This record contains composition relationships requiring review; no cold-heading suitability or strength-class recommendation is provided to customers.

G12144 · ASTM A29/A29M-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Spring steels
Subcategory
Spring steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.85 ~ 1.15
P0.04 ~ 0.09
Pb0.15 ~ 0.35
S0.26 ~ 0.35

Applicability and limitations

This record contains composition relationships requiring review; no cold-heading suitability or strength-class recommendation is provided to customers.

G12144 · ASTM A29/A29M-2023

Original-source verification is incomplete; this is not a formal standard reference

Material category
Spring steels
Subcategory
Spring steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Mn0.85 ~ 1.15
P0.04 ~ 0.09
Pb0.15 ~ 0.35
S0.26 ~ 0.35

Applicability and limitations

This record contains composition relationships requiring review; no cold-heading suitability or strength-class recommendation is provided to customers.