- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Original record status
- Reference data; original source not verified
- Standard edition
- SAE J403-2014
- Table / clause
- Table 1
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Flat products, within the scope of Table 1/2 and note 1
Long products, within the scope of Table 1/2 and note 1; The scope of Table 2 is not extended to wire rod on this basis
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.28 ~ 0.34 |
| Mn | 0.6 ~ 0.9 |
| B | 0.0005 ~ 0.003 |
Applicability and limitations
P and S shall be selected separately according to flat products/long products; Upper limits cannot be combined. ; Si requires agreement at ordering: wire rod options are ≤0.10, 0.07–0.15, 0.10–0.20, 0.15–0.35, 0.20–0.40, 0.30–0.60%.; Other products have the same options as listed, except for 0.07–0.15. Fixed Si shall not be entered if not agreed. ; Residual elements Note 2: A Cu≤0.20/Ni≤0.20/Cr≤0.15/Mo≤0.06; B Cu≤0.35/Ni≤0.25/Cr≤0.20/Mo≤0.06 (default when not otherwise agreed); C Cu≤0.40/Ni≤0.40/Cr≤0.30/Mo≤0.12; Option D has no specified limits, but reporting is required.. Option A applies to flat products in grades ≤1060; other cases require agreement.. ; Note 3: For boron steels, insert B between the second and third positions, and change the last digit of the UNS to 1; B is 0.0005–0.003%.
Original condition-branch records
Flat products, within the scope of Table 1/2 and note 1
| Element | Composition requirement |
|---|---|
| C | 0.28 ~ 0.34 |
| Mn | 0.6 ~ 0.9 |
| B | 0.0005 ~ 0.003 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
Long products, within the scope of Table 1/2 and note 1; The scope of Table 2 is not extended to wire rod on this basis
| Element | Composition requirement |
|---|---|
| C | 0.28 ~ 0.34 |
| Mn | 0.6 ~ 0.9 |
| B | 0.0005 ~ 0.003 |
| P | ≤ 0.04 (lower limit not stated) |