ELCH2 · Kobe Steel manufacturer specification (section 6-6)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Soft magnetic materials
Subcategory
Soft magnetic materials
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-6
PDF page references
27
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel
Classification basis (does not replace original-source composition verification)

Reuse the verified soft-magnetic-material application in Kobe Steel catalogue Section 6-6 (PDF page 27); No standard guarantee for electromagnetic pure iron or supply by Creation Group is claimed.

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.03 (lower limit not stated)
Mn0.2 ~ 0.3
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
Ni≤ 0.15 (lower limit not stated)
Cr≤ 0.15 (lower limit not stated)

Applicability and limitations

Original composition for soft magnetic materials in the Kobe Steel catalogue, section 6-6 (PDF page 27), mass fractions wt%; This is not the original JIS/SAE standard. The manufacturer catalogue does not state a publication year; actual supply and application require separate confirmation; This does not establish a supply commitment from Creation Group.

Composition conditions

Verification notes

The original manufacturer catalogue table was checked cell by cell against the boundaries of the PDF table; Added elements without numerical values are retained as text only.