← BackMaterial grade directory

E335

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for E335 →

E335 · EN 10025-2-2019

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10025-2-2019
Table / clause
Table 2 default heat analysis and 7.2.1; The special increased-sulfur condition is not enabled
PDF page references
1、12、24

Carbon-equivalent reference

IIW / CEV:0.0000–0.4177Known-element contribution; incomplete value; missing C CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.1618Known-element contribution; incomplete value; missing C Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.2155Known-element contribution; incomplete value; missing C CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
Al≤ 0.3 (lower limit not stated)
B≤ 0.0008 (lower limit not stated)
Bi≤ 0.1 (lower limit not stated)
Co≤ 0.3 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Cu≤ 0.4 (lower limit not stated)
Mn≤ 1.65 (lower limit not stated)
Mo≤ 0.08 (lower limit not stated)
Nb≤ 0.06 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)
Pb≤ 0.4 (lower limit not stated)
Se≤ 0.1 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)
Te≤ 0.1 (lower limit not stated)
Ti≤ 0.05 (lower limit not stated)
V≤ 0.1 (lower limit not stated)
W≤ 0.3 (lower limit not stated)
Zr≤ 0.05 (lower limit not stated)
O≤ 0.1 (lower limit not stated)
Sn≤ 0.1 (lower limit not stated)
As≤ 0.1 (lower limit not stated)
Sb≤ 0.1 (lower limit not stated)
Mg≤ 0.1 (lower limit not stated)
Zn≤ 0.1 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.045 (lower limit not stated)
N≤ 0.012 (lower limit not stated)

Applicability and limitations

EN10025-2:2019 Table 2 heat analysis: P≤.045%, S≤.045%, N≤.012%; FN does not allow rimmed steel. ; Carbon range is not specified in this table and shall not be copied from other grades; Complete calculation results for carbon equivalent cannot be provided when C is missing. ; For elements not defined, 7.2.1 refers to the upper limits in EN10020:2000 Table 1.; Do not invent unlisted ranges for C/P/S/N. ; Table 2, Note c raises S by .010 for long products with improved machinability, whereas Clause 13, Option 27 states .015; the discrepancy is retained.; Special increase in S is not open; ordinary table values are retained.. ; Table 2, Note d: The N upper limit need not apply when total Al≥.020% or sufficient other nitrogen-fixing elements are present, with the condition recorded in the inspection certificate.; This condition shall be selected after verification. ; Standard CEV upper limits in Table 5 are listed only for S235/S275/S355/S460/S500 and shall not be applied to E295/E335/E360. ; Reference for hot-rolled structural steel materials; cold-heading process and supply applicability shall be verified separately; Not automatically added to product center.

Combined limits

Nitrogen-fixing exception conditions
Yes

Verification notes

Ordinary composition and references in Table 2 have been checked; Differences in the special increased-S provision still require verification

E335 · EN 10025-2-2019

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10025-2-2019
Table / clause
Table 2 default heat analysis and 7.2.1; The special increased-sulfur condition is not enabled
PDF page references
1、12、24

Carbon-equivalent reference

IIW / CEV:0.0000–0.4177Known-element contribution; incomplete value; missing C CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.1618Known-element contribution; incomplete value; missing C Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.2155Known-element contribution; incomplete value; missing C CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
Al≤ 0.3 (lower limit not stated)
B≤ 0.0008 (lower limit not stated)
Bi≤ 0.1 (lower limit not stated)
Co≤ 0.3 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Cu≤ 0.4 (lower limit not stated)
Mn≤ 1.65 (lower limit not stated)
Mo≤ 0.08 (lower limit not stated)
Nb≤ 0.06 (lower limit not stated)
Ni≤ 0.3 (lower limit not stated)
Pb≤ 0.4 (lower limit not stated)
Se≤ 0.1 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)
Te≤ 0.1 (lower limit not stated)
Ti≤ 0.05 (lower limit not stated)
V≤ 0.1 (lower limit not stated)
W≤ 0.3 (lower limit not stated)
Zr≤ 0.05 (lower limit not stated)
O≤ 0.1 (lower limit not stated)
Sn≤ 0.1 (lower limit not stated)
As≤ 0.1 (lower limit not stated)
Sb≤ 0.1 (lower limit not stated)
Mg≤ 0.1 (lower limit not stated)
Zn≤ 0.1 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.045 (lower limit not stated)
N≤ 0.012 (lower limit not stated)

Applicability and limitations

EN10025-2:2019 Table 2 heat analysis: P≤.045%, S≤.045%, N≤.012%; FN does not allow rimmed steel. ; Carbon range is not specified in this table and shall not be copied from other grades; Complete calculation results for carbon equivalent cannot be provided when C is missing. ; For elements not defined, 7.2.1 refers to the upper limits in EN10020:2000 Table 1.; Do not invent unlisted ranges for C/P/S/N. ; Table 2, Note c raises S by .010 for long products with improved machinability, whereas Clause 13, Option 27 states .015; the discrepancy is retained.; Special increase in S is not open; ordinary table values are retained.. ; Table 2, Note d: The N upper limit need not apply when total Al≥.020% or sufficient other nitrogen-fixing elements are present, with the condition recorded in the inspection certificate.; This condition shall be selected after verification. ; Standard CEV upper limits in Table 5 are listed only for S235/S275/S355/S460/S500 and shall not be applied to E295/E335/E360. ; Reference for hot-rolled structural steel materials; cold-heading process and supply applicability shall be verified separately; Not automatically added to product center.

Combined limits

Nitrogen-fixing exception conditions
Yes

Verification notes

Ordinary composition and references in Table 2 have been checked; Differences in the special increased-S provision still require verification

E335 · DIN EN 10025-2-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
N≤ 0.012 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.045 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →