E295
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for E295 →E295 · EN 10025-2-2019
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10025-2-2019
- Table / clause
- Table 2 default heat analysis and 7.2.1; The special increased-sulfur condition is not enabled
- PDF page references
- 1、12、24
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | ≤ 0.3 (lower limit not stated) |
| B | ≤ 0.0008 (lower limit not stated) |
| Bi | ≤ 0.1 (lower limit not stated) |
| Co | ≤ 0.3 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Cu | ≤ 0.4 (lower limit not stated) |
| Mn | ≤ 1.65 (lower limit not stated) |
| Mo | ≤ 0.08 (lower limit not stated) |
| Nb | ≤ 0.06 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Pb | ≤ 0.4 (lower limit not stated) |
| Se | ≤ 0.1 (lower limit not stated) |
| Si | ≤ 0.6 (lower limit not stated) |
| Te | ≤ 0.1 (lower limit not stated) |
| Ti | ≤ 0.05 (lower limit not stated) |
| V | ≤ 0.1 (lower limit not stated) |
| W | ≤ 0.3 (lower limit not stated) |
| Zr | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.1 (lower limit not stated) |
| Sn | ≤ 0.1 (lower limit not stated) |
| As | ≤ 0.1 (lower limit not stated) |
| Sb | ≤ 0.1 (lower limit not stated) |
| Mg | ≤ 0.1 (lower limit not stated) |
| Zn | ≤ 0.1 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.045 (lower limit not stated) |
| N | ≤ 0.012 (lower limit not stated) |
Applicability and limitations
EN10025-2:2019 Table 2 heat analysis: P≤.045%, S≤.045%, N≤.012%; FN does not allow rimmed steel. ; Carbon range is not specified in this table and shall not be copied from other grades; Complete calculation results for carbon equivalent cannot be provided when C is missing. ; For elements not defined, 7.2.1 refers to the upper limits in EN10020:2000 Table 1.; Do not invent unlisted ranges for C/P/S/N. ; Table 2, Note c raises S by .010 for long products with improved machinability, whereas Clause 13, Option 27 states .015; the discrepancy is retained.; Special increase in S is not open; ordinary table values are retained.. ; Table 2, Note d: The N upper limit need not apply when total Al≥.020% or sufficient other nitrogen-fixing elements are present, with the condition recorded in the inspection certificate.; This condition shall be selected after verification. ; Standard CEV upper limits in Table 5 are listed only for S235/S275/S355/S460/S500 and shall not be applied to E295/E335/E360. ; Reference for hot-rolled structural steel materials; cold-heading process and supply applicability shall be verified separately; Not automatically added to product center.
Combined limits
- Nitrogen-fixing exception conditions
- Yes