E1524H
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for E1524H →E1524H · SAE J1268-2010
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- SAE J1268-2010
- Table / clause
- Table 1 and Notes 1/2; Clause 3
- PDF page references
- 1、2、3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.18 ~ 0.26 |
| Mn | 1.21 ~ 1.75 |
| Si | 0.15 ~ 0.35 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
Applicability and limitations
SAE J1268 MAY2010 official English original Table 1, ladle analysis mass fraction wt%, H-steel hardenability band materials. ; Table 1 Note 1: When electric furnace melting is specified or required, the grade shall have an E prefix, P/S each ≤.025%, and shall be separated from ordinary H grades. ; Table 1 Note 2 Boron steel B .0005–.003%; Unlisted residual alloying elements shall not be arbitrarily matched to J403/J404 values; unspecified elements shall not be assumed zero. ; The permissible composition range for H-steels is established to satisfy the hardenability band and shall not be merged with grades of the same name without H. ; Finished product analysis tolerances must be separately determined according to SAE J409 Table 1/3; Hardenability curves, grain size, delivery conditions, and cold heading supply shall be separately verified.