DT4A · GB/T 6983-2022

Original-source verification is incomplete; this is not a formal standard reference

Material category
Other metallic materials
Material form
Electromagnetic pure iron (source classification)
Verification status
Original standard verified
Standard edition
GB/T 6983-2022
Table / clause
Main text: Table 2, row 2; Informative Annex A · Table A.1
PDF page references
6、10
Unit
Mass fraction (%)
Analysis type
Informative-annex reference

Carbon-equivalent reference

Composition from an informative standard annex is for reference only. Normative composition and edition remain unverified; standard-range carbon equivalents and reverse matching are disabled.

Composition

ElementComposition requirement
C≤ 0.006 (lower limit not stated)
Si≤ 0.08 (lower limit not stated)
Mn≤ 0.25 (lower limit not stated)
P≤ 0.012 (lower limit not stated)
S≤ 0.006 (lower limit not stated)
Al≤ 0.8 (lower limit not stated)
Ti≤ 0.005 (lower limit not stated)
Cr≤ 0.03 (lower limit not stated)
Ni≤ 0.02 (lower limit not stated)
Cu≤ 0.02 (lower limit not stated)

Applicability and limitations

GB/T 6983—2022, main-text Table 2, row 2: DT4A is the high electromagnetic-performance class; For specimens annealed as specified: coercivity Hc≤60 A/m, aging increment ≤6 A/m, and maximum permeability ≥0.0100 H/m; Minimum B200/B500/B1000/B2500/B5000/B10000 magnetic flux densities (T) are, in order, 1.20, 1.40, 1.50, 1.62, 1.71 and 1.80. These electromagnetic properties apply under the specified specimen treatment and test conditions and are not guarantees for arbitrary delivery conditions. Main-text 7.1 requires chemical analysis to be provided but does not use it as a delivery-acceptance criterion; Chemical composition is transcribed only from the common reference values in informative Annex A, Table A.1; these are not independent mandatory composition limits for the four grades. Product dimensions and form must be confirmed under main-text Table 1 and the order contract.

Verification notes

Grade designations and electromagnetic classes in main-text Table 2 have been checked; Annex A composition is informative reference only