← BackMaterial grade directory

DD402

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for DD402 →

DD402 · GB /T 14992-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Ag≤ 0.0005 (lower limit not stated)
Al5.45 ~ 5.75
As≤ 0.0005 (lower limit not stated)
B≤ 0.003 (lower limit not stated)
Bi≤ 3e-05 (lower limit not stated)
C≤ 0.006 (lower limit not stated)
Co4.3 ~ 4.9
Cr7 ~ 8.2
Cu≤ 0.05 (lower limit not stated)
Fe≤ 0.2 (lower limit not stated)
Ga≤ 0.002 (lower limit not stated)
Mg≤ 0.008 (lower limit not stated)
Mn≤ 0.02 (lower limit not stated)
Mo0.3 ~ 0.7
N≤ 0.0012 (lower limit not stated)
Nb≤ 0.15 (lower limit not stated)
O≤ 0.001 (lower limit not stated)
P≤ 0.005 (lower limit not stated)
Pb≤ 0.0002 (lower limit not stated)
S≤ 0.002 (lower limit not stated)
Sb≤ 0.0005 (lower limit not stated)
Se≤ 0.0001 (lower limit not stated)
Si≤ 0.04 (lower limit not stated)
Sn≤ 0.0015 (lower limit not stated)
Ta5.8 ~ 6.2
Ti0.8 ~ 1.2
W7.6 ~ 8.4
Zn≤ 0.0005 (lower limit not stated)
Zr≤ 0.0075 (lower limit not stated)

Applicability and limitations

This record contains composition relationships requiring review; no cold-heading suitability or strength-class recommendation is provided to customers.

DD402 · GB /T 14992-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Special alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Ag≤ 0.0005 (lower limit not stated)
Al5.45 ~ 5.75
As≤ 0.0005 (lower limit not stated)
B≤ 0.003 (lower limit not stated)
Bi≤ 3e-05 (lower limit not stated)
C≤ 0.006 (lower limit not stated)
Co4.3 ~ 4.9
Cr7 ~ 8.2
Cu≤ 0.05 (lower limit not stated)
Fe≤ 0.2 (lower limit not stated)
Ga≤ 0.002 (lower limit not stated)
Mg≤ 0.008 (lower limit not stated)
Mn≤ 0.02 (lower limit not stated)
Mo0.3 ~ 0.7
N≤ 0.0012 (lower limit not stated)
Nb≤ 0.15 (lower limit not stated)
O≤ 0.001 (lower limit not stated)
P≤ 0.005 (lower limit not stated)
Pb≤ 0.0002 (lower limit not stated)
S≤ 0.002 (lower limit not stated)
Sb≤ 0.0005 (lower limit not stated)
Se≤ 0.0001 (lower limit not stated)
Si≤ 0.04 (lower limit not stated)
Sn≤ 0.0015 (lower limit not stated)
Ta5.8 ~ 6.2
Ti0.8 ~ 1.2
W7.6 ~ 8.4
Zn≤ 0.0005 (lower limit not stated)
Zr≤ 0.0075 (lower limit not stated)

Applicability and limitations

This record contains composition relationships requiring review; no cold-heading suitability or strength-class recommendation is provided to customers.