CM30
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for CM30 →Cm30 · DIN 17200-1987
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN 17200-1987-03
- Table / clause
- Table 2 and footnotes 1–5; 7.3.1–7.3.2
- PDF page references
- 1、2、15、16、17
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.27 ~ 0.34 |
| Mn | 0.5 ~ 0.8 |
| Si | ≤ 0.4 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | 0.02 ~ 0.035 |
Applicability and limitations
Table 2 cast analysis, mass fraction wt%; Si is an upper limit and unspecified elements are not filled with zero. P/S requirements for the C, Ck and Cm series remain separate; S 0.020–0.035% in S-containing grades is a two-sided range. Note 1: unlisted elements may not be intentionally added without purchaser consent, except to complete melting; no fixed residual values are inferred. Table 3 contains permissible product-analysis deviations, not added to cast limits; applicable sizes and positive/negative directions are checked separately. Heat-treatment condition, hardenability and size-dependent properties require separate verification. The standard includes hot-rolled wire rod; chemistry alone is no cold-heading supply commitment. Note 2: small composition deviations, excluding P/S, may be agreed when ordering restricted hardenability bands or quenched-and-tempered/normalized properties, but may not exceed Table 3. These data retain the Table 2 baseline without automatic relaxation. Light-typeface grades in note 4 are for special applications only. Note 5 permits separate ordering of Pb 0.15–0.30% only for the marked C-series grades; not added to ordinary base compositions. Original material number 1.1179; Note 4: special applications only.