C60R · DIN EN 10277:2018-09

Original table in an informative annex verified; normative composition requirements and edition still require verification. For reference only.

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Composition basis
Heat analysis in an informative annex; for reference only
Verification status
Original table in an informative annex verified; normative composition requirements and edition still require verification
Standard edition
DIN EN 10277:2018-09
Table / clause
Informative Annex A.4
PDF page references
46
Unit
mass fraction (wt%)
Analysis type
Heat analysis (informative reference)

Carbon-equivalent reference

Composition from an informative standard annex is for reference only. Normative composition and edition remain unverified; standard-range carbon equivalents and reverse matching are disabled.

Composition

ElementComposition requirement
C0.57 ~ 0.65
Si0.1 ~ 0.4
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.04
Cr≤ 0.4 (lower limit not stated)
Mo≤ 0.1 (lower limit not stated)
Ni≤ 0.4 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

The original informative-annex table has been checked and is for reference only. Clause 7.1.2 requires chemical composition to be determined under the cited standard; the formal normative composition and applicable edition remain unverified. Do not use it as a delivery guarantee, a reverse-search acceptance criterion or a basis for standard-range carbon equivalent.

Composition conditions

Combined limits

Element-sum limits
  • Elements concerned
    • Cr
    • Mo
    • Ni
    Upper limit
    0.63
    Additional source notes
    Cr+Mo+Ni: 0,63

Conditional requirement

Verification notes

The original informative-annex table has been checked and is for reference only. Clause 7.1.2 requires chemical composition to be determined under the cited standard; the formal normative composition and applicable edition remain unverified. Do not use it as a delivery guarantee, a reverse-search acceptance criterion or a basis for standard-range carbon equivalent.