C17GC
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for C17GC →C17GC · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Cold-heading wire
- Original record status
- Reference transcription of standard
- Standard edition
- ISO 4954:2018
- Table / clause
- Table A.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.19 |
| Si | 0.15 ~ 0.25 |
| Mn | 0.65 ~ 0.85 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Cr+Ni+Mo | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018; Heat analysis, mass percent; Values without stated ranges are maxima; See the original page for the complete table notes. No edition is stated on the website; Displayed under this source edition; contract applicability is not established; ISO4954:2018 Table A.2 applies to steels not intended for heat treatment after cold working, heat analysis wt%; The original text specifies Cr+Ni+Mo total ≤0.50%; in addition to individual element limits, the total must also be satisfied; Elements not entered shall remain unknown and not be treated as 0; Optional deoxidation/aluminum substitution and Mn agreements shall still be verified against explicit ordering conditions.
Combined limits
- Element-sum limits
- Elements concerned
- Cr
- Ni
- Mo
- Upper limit
- 0.5
Verification notes
Standard source: ISO 4954:2018 · Table A.2View associated products →C17GC · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Steel not heat-treated after cold working
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ISO 4954:2018
- Table / clause
- Table A.2
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Note c, quality a: Al≤0.015%
Note c, quality b: no addition of Al, Si0.15–0.25%; No intentional addition does not mean an analyzed content of 0
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.19 |
| Si | 0.15 ~ 0.25 |
| Mn | 0.65 ~ 0.85 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018, Table A.2 gives heat analysis; A single value is a maximum; a dash is not zero. ; Product-analysis tolerances are listed separately under Table 2/3 of the standard and do not directly widen the heat-analysis composition ranges. ; Applicable to steels that do not undergo heat treatment after cold working. ; Al may be replaced by other elements with similar effects; Al cannot be required to reach the lower limit listed in the table without conditions. ; A lower Mn may be specified for C2C/C20C/C20GC/C25C, with a range width of 0.20%; Subject to ordering agreement. ; Note c Two quality levels: Al ≤0.015%; Alternatively, no Al addition and Si 0.15–0.25% for hot-dip galvanizing.. Apply after selection.
Combined limits
- Element-sum limits
- Elements concerned
- Cr
- Ni
- Mo
- Upper limit
- 0.5
- Conditional composition lower limit
- Al
- Applicable conditions
- May be replaced by other elements with a similar effect
Original condition-branch records
Note c, quality a: Al≤0.015%
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.19 |
| Si | 0.15 ~ 0.25 |
| Mn | 0.65 ~ 0.85 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |
| Al | ≤ 0.015 (lower limit not stated) |
Note c, quality b: no addition of Al, Si0.15–0.25%; No intentional addition does not mean an analyzed content of 0
| Element | Composition requirement |
|---|---|
| C | 0.15 ~ 0.19 |
| Si | 0.15 ~ 0.25 |
| Mn | 0.65 ~ 0.85 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | ≤ 0.3 (lower limit not stated) |
| Ni | ≤ 0.3 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.3 (lower limit not stated) |