← BackMaterial grade directory

BZN18-20

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for BZN18-20 →

BZn18-20 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 5, row 29, designation T76300
PDF page references
12
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Fe≤ 0.3 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
Pb≤ 0.03 (lower limit not stated)
Al≤ 0.005 (lower limit not stated)
Si≤ 0.15 (lower limit not stated)
P≤ 0.005 (lower limit not stated)
S≤ 0.005 (lower limit not stated)
C≤ 0.03 (lower limit not stated)
Sn≤ 0.08 (lower limit not stated)
Bi≤ 0.002 (lower limit not stated)
Ti≤ 0.005 (lower limit not stated)
Sb≤ 0.002 (lower limit not stated)
Cu60.0 ~ 63.0

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 5, row 29, designation T76300; scanned PDF, PDF physical page 12. Cu follows the table range, and Zn is balance. Ni+Co is a combined range and must not be split into individual Ni or Co limits. Dashes mean unspecified and are not replaced with zero. Total table-listed impurities ≤0.8%, subject to the applicable table notes. This standard provides the grade-composition basis for wrought copper-nickel alloys; actual supply and cold-heading suitability require separate confirmation. Note d to Table 5: total impurities means the sum of measured values for the impurity elements listed in the table. Note a to Table 5: analysis of Bi, Sb and As may be omitted, but the supplier must ensure that their contents do not exceed the limits.

Combined limits

Combined-element limits
  • Requirement
    Table 5: Ni+Co total
    Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    16.5
    Upper limit
    19.5
Elements requiring measured values from the same heat
  • Ni
  • Co

Verification notes

Manual cell-by-cell check of Table 5 in the scanned standard original; cross-column elements, summed compositions and footnotes were checked.
WhatsApp Technical enquiry →