2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for BMN3-12 →

BMn3-12 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 4 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Fe0.2 ~ 0.5
Mn11.5 ~ 13.5
Pb≤ 0.02 (lower limit not stated)
Al≤ 0.2 (lower limit not stated)
Si0.1 ~ 0.3
P≤ 0.005 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Mg≤ 0.03 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Cu is the balance. Note 3: departures of the relevant extrema from Table 4 are permitted to ensure electrical properties, subject to confirmation of the conditions; This record retains the tabulated baseline. Note 1: Bi/As/Sb need not be analyzed; the supplier guarantees that the limit is not exceeded.

Combined limits

Combined-element limits
  • Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    2.0
    Upper limit
    3.5
    Requirement
    Total Ni + Co
Elements requiring measured values from the same heat
  • Co
  • Ni

Verification notes

The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.

BMn3-12 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 5, row 16, designation T71620
PDF page references
11
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al≤ 0.2 (lower limit not stated)
Fe0.2 ~ 0.5
Mn11.5 ~ 13.5
Pb≤ 0.02 (lower limit not stated)
P≤ 0.005 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
C≤ 0.05 (lower limit not stated)
Mg≤ 0.03 (lower limit not stated)
Si0.1 ~ 0.3

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 5, row 16, designation T71620; Scanned PDF, page 11. Cu is the balance. Ni+Co is a combined range and must not be split into independent Ni or Co ranges; A dash means unspecified; it is not entered as zero. Tabulated total impurities ≤0.5%, verified under the applicable table notes. This standard provides designation and composition requirements for wrought copper-nickel alloys; actual supply and cold-heading suitability require separate confirmation. Table 5, note c: for thermocouple applications, slight departures from specified composition maxima or minima are permitted to ensure electrical properties; Applicability must be confirmed separately for the intended use.

Combined limits

Combined-element limits
  • Requirement
    Table 5: Ni+Co total
    Element coefficient
    Ni
    1
    Co
    1
    Lower limit
    2.0
    Upper limit
    3.5
Elements requiring measured values from the same heat
  • Ni
  • Co

Verification notes

Manual cell-by-cell check of Table 5 in the scanned standard original; cross-column elements, summed compositions and footnotes were checked.